Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL GTX™ Resin GTX985 - Asia - (PPE+PA*)-MF18 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL GTX™ Resin GTX985 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl GTX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
NORYL GTX™ 985 resin is a conductive, 18% mineral reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade combines high stiffness, excellent chemical resistance, and high heat resistance. NORYL GTX985 is conductive for primerless electrostatic painting and is an excellent candidate for automotive exterior trim applications.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 15 cm³/10min ISO 1133
温度 280 °C -
荷重 5 kg -
ASTM数据
メルトフローレイト, MFI 16 g/10min ASTM D 1238
温度 280 °C -
荷重 5 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 4400 MPa ISO 527
降伏応力 65 MPa ISO 527
降伏ひずみ 4 % ISO 527
破壊応力 60 MPa ISO 527
破壊ひずみ 7 % ISO 527
曲げ弾性率 4350 MPa ISO 178
ノッチ付きシャルピー衝撃強さ, +23°C 4 kJ/m² ISO 179/1eA
アイゾット衝撃試験, +23°C 60 kJ/m² ISO 180/1U
ノッチ付きアイゾット衝撃強さ, +23°C, 4mm 4 kJ/m² ISO 180/1A
ノッチ付きアイゾット衝撃強さ, -30°C, 4mm 4 kJ/m² ISO 180/1A
ASTM数据
降伏応力 65 MPa ASTM D 638
破壊応力 60 MPa ASTM D 638
降伏点伸び 4 % ASTM D 638
破断伸び 7 % ASTM D 638
曲げ弾性率 4200 MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 45 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 40 J/m ASTM D 256
温度 -30 °C -
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 0.45 MPa 205 °C ISO 75-1/-2
ビカット軟化温度, B 195 °C ISO 306
ビカット軟化温度, 120°C/h 50N 200 °C ISO 306
線膨張係数, 平行 60 E-6/K ISO 11359-1/-2
線膨張係数, 直角 65 E-6/K ISO 11359-1/-2
ASTM数据
DTUL @ 66 psi 200 °C ASTM D 648
ビカット軟化温度 195 °C ASTM D 1525
その他の特性.単位テスト基準
吸湿率 1.1 % Sim. to ISO 62
密度. 1250 kg/m³ ISO 1183
密度 1250 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 100 - 110 °C -
Pre-drying - Time 2 - 3 h -
Processing humidity ≤0.02 % -
樹脂温度 280 - 300 °C -
金型温度 100 - 120 °C -
Feed temperature 80 - 100 °C -
Zone 1 260 - 280 °C -
Zone 2 270 - 290 °C -
Zone 3 280 - 300 °C -
特殊な特性
成形加工法.
射出成形.
アプリケーション
自動車
領域別の利用可能性
アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.